— Typical copper electrolyte solution produced from leaching of copper ore, contains 25–60 g/L of copper and 0.1–10 g/L of iron in the electrowinning stage (Evans, 2003; Habashi, 1998). These industrial processes operate in temperatures of 40–60 °C, pH of 1 and current densities in the range of 20–45 mA/cm 2 are used ( Moats and Free ...