Thus, cryogenic grinding resulted in 29.5% more volatile oil in comparison to that of ambient grinding. When grinding temperature was increased from −110 to −50C, there were increases in particle size for the same cumulative volume fraction. the volume mean diameter of clove powder increased quadratically from 119 to 153 μm with increases ...