ABSTRACT Hematite pellet is required to be indurated at very high temperature to achieve its good strength as there is no exothermic heat of oxidation unlike magnetite. As mill scale contains mainly FeO and Fe3O4, any minor amount of its addition in pellet can provide in situ heat and enhance diffusion bonding and sintering. In this study, the mill scale …